高压凝固Mg-xAl (x = 3, 5, 7, 9, 12)合金组织结构及耐腐蚀性能 |
| 郭耀威, 艾士民, 房大然, 林小娉, 杨连威, 郑哲皓 |
|
Microstructure and Corrosion Resistance of High-pressure Solidified Mg-xAl (x = 3, 5, 7, 9, 12) Alloys |
| GUO Yaowei, AI Shimin, FANG Daran, LIN Xiaoping, YANG Lianwei, ZHENG Zhehao |
| 图6 Mg-xAl (x = 3,5,7,9,12)合金的极化曲线及Ecorr与Icorr随Al含量的变化 |
| Fig.6 Polarization curves of conventional cast (a) and high-pressure solidified (b) Mg-xAl (x = 3, 5, 7, 9, 12) alloys, variations of corrosion potential (Ecorr) and corrosion current density (Icorr) with Al content (c) |
|