大气等离子热障涂层体系在900 ℃含水蒸气和NaCl环境下的腐蚀行为 |
李琰琰, 李帅, 董超, 李冬强, 鲍泽斌, 朱圣龙 |
Corrosion Behavior of Atmospheric Plasma Spray Thermal Barrier Coatings at 900 °C Beneath NaCl Deposits in Oxygen Flow Carrying Water Vapor |
LI Yanyan, LI Shuai, DONG Chao, LI Dongqiang, BAO Zebin, ZHU Shenglong |
图7 Praxair 7700喷涂制备YSZ热障涂层体系腐蚀100和200 h后的微观截面形貌 |
Fig.7 Cross-sectional morphologies of TBC with the YSZ top coating deposited by Praxair 7700 after corrosion for 100 h (a, b) and 200 h (c, d) |
![]() |