沉淀相对镍基718合金高温高压水环境应力腐蚀裂纹萌生行为影响研究 |
李维鹏, 罗坤杰, 王惠生, 陈嘉诚, 韩姚磊, 庞晓露, 彭群家, 乔利杰 |
Effect of Precipitation on Stress Corrosion Cracking Initiation of Nickel Based 718 Alloy in High Temperature and High Pressure Water |
LI Weipeng, LUO Kunjie, WANG Huisheng, CHEN Jiacheng, HAN Yaolei, PANG Xiaolu, PENG Qunjia, QIAO Lijie |
图5 高温高压水环境镍基718合金B种带材SSRT实验原位SEM观察及EDS分析结果 |
Fig.5 In-situ SEM observation and EDS analysis of B type of 718 alloy strips during SSRT experiment in high-temperature and high-pressure water environment, showing the presence of cracks at different strains (a-c) and compositions of (Nb, Ti)C (d) in Fig.5a2 and TiN (e) in Fig.5a3 precipitation phases |
![]() |