3.5%NaCl溶液中硝基巴比妥酸对AZ31BAZ91D镁合金腐蚀的缓蚀作用及机理研究
翟亚如, 熊金平, 赵景茂

Corrosion Inhibition Performance of Nitrobarbituric Acid on Mg-alloys AZ31B and AZ91D in 3.5%NaCl Solution
ZHAI Yaru, XIONG Jinping, ZHAO Jingmao
表5 AZ31B在25 ℃添加和不添加1 g/L NBA的3.5%NaCl溶液中EIS拟合参数
Table 5 Fitting parameters of AZ31B in 3.5%NaCl solution with or without 1 g/L NBA at 25 ℃
Corrosion inhibitorRsΩ·cm2QfΩ-1·cm-2·s nnRfΩ·cm2RLΩ·cm2LH·cm2CdlΩ-1·cm-2·s nRctΩ·cm2χ2
Blank55.78---2.172 × 1023.114 × 1022.679 × 10-51.166 × 1021.210 × 10-3
NBA82.902.725 × 10-50.79011.582 × 103--6.743 × 10-62.686 × 1043.129 × 10-3