海上超临界二氧化碳环境中含水率和温度对A106钢腐蚀行为影响研究
张国庆, 余直霞, 王岳松, 王智, 金正宇, 刘宏伟

Corrosion Behavior of Steel Materials in Marine Supercritical Carbon Dioxide Environment
ZHANG Guoqing, YU Zhixia, WANG Yuesong, WANG Zhi, JIN Zhengyu, LIU Hongwei
图4 A106钢在35 ℃不同含水量的超临界CO2环境中暴露5 d后表面腐蚀产物XRD分析结果
Fig.4 XRD analysis results of the corrosion products formed on A106 steel exposed at 35 ℃ for 5 d in sc-CO2 environments containing 200 μL/L (a), 1000 μL/L (b), 1500 μL/L (c), 2000 μL/L (d), 2500 μL/L (e) and 3000 μL/L (f) H2O