7075-T6铝合金在3.5%NaCl溶液中的摩擦腐蚀性能研究 |
| 杜晋, 胡林岚, 孙健, 宋庆华, 陈蒙, 肖金坤 |
|
Tribo-corrosion Performance of 7075-T6 Al-alloy in 3.5%NaCl Solution |
| DU Jin, HU Linlan, SUN Jian, SONG Qinghua, CHEN Meng, XIAO Jinkun |
| 图1 摩擦腐蚀实验装置图 |
| Fig.1 Diagram of tribocorrosion testing device: (a) experimental setup diagram, (b) local diagram of the tribocorrosion device |
|