RGO-CNTs杂化材料改性RuO2-IrO2-SnO2/Ti阳极的性能研究
赵菲, 王东伟, 郭泉忠, 汪川

Performance of RGO-CNTs Hybrid Material Modified RuO2-IrO2-SnO2/Ti Anode
ZHAO Fei, WANG Dongwei, GUO Quanzhong, WANG Chuan
表3 3.5%NaCl溶液中不同金属氧化物阳极的电化学阻抗谱拟合数据
Table 3 Electrochemical impedance spectroscopy fitting data of different metal oxide anodes in 3.5%NaCl solution
ElectrodeRs / Ω·cm2Qf / Ω-1·cm-2·s nnRf / Ω·cm2Qdl / Ω-1·cm-2·s nnRct / Ω·cm2
N17.1140.18760.711418.940.002620.701921.43
H17.1940.19980.777213.620.005810.685711.48
N27.0190.15440.213222.380.002080.868013.91
H27.5470.16860.124712.420.004240.79487.35
N37.4370.02570.334142.630.001950.812632.35
H37.1510.13460.16819.230.000970.822727.95