高速列车用铝合金环氧底漆的腐蚀行为和湿热老化机理研究
|
|
李丽, 李善文, 史洪微, 梁国平, 李春霖, 孙禹, 秦晋, 王伟, 韩恩厚
|
Corrosion Behavior and Hydrothermal Aging Mechanism of Epoxy Primer on Al-alloy for High-speed Train
|
|
LI Li, LI Shanwen, SHI Hongwei, LIANG Guoping, LI Chunlin, SUN Yu, QIN Jin, WANG Wei, HAN En-Hou
|
|
表2 环氧树脂中主要官能团的FTIR峰
|
Table 2 FTIR peaks of main functional groups in epoxy resin
|
|
| Vibration mode of functional groups | Vibration frequency / cm-1 |
|---|
| O-H stretching N-H stretching | 3296 | | Asymmetric -CH2 stretching | 2923 | | Symmetric -CH2 stretching | 2852 | | C=O stretching | 1720 | | C=O stretching in amide | 1642 | | C=C stretching in benzene ring | 1606、1507、1181 | | C=C stretching | 1582 | | -CH3 bending | 1456 | | C-N stretching | 1296 | | Asymmetric C-O-φ stretching | 1237 (φ represents benzene ring) | | Symmetric C-O-φ stretching | 1034 | | C-O-C stretching | 1011 | | Para-substituted of benzene ring stretching in bisphenol A structure | 879、826 |
|
|
|