图13 焊接接头(TIG,MAG以及EBW)和基体金属在80 ℃、人工海水饱和的无氧膨润土中腐蚀3年的平均腐蚀速率[66]
Fig.13 Corrosion rates of the weld joints (TIG, MAG, and EBW) and base metal after embedding in compacted bentonite saturated with synthetic sea water at 80 ℃ for 3 a[66]