日本高放废物处置容器腐蚀厚度设计研究进展
彭立园, 谢敬礼, 曹胜飞, 谭季波, 吴欣强, 张兹瑜

Review on Corrosion Thickness Design of Canister for High-level Radioactive Waste in Japan
PENG Liyuan, XIE Jingli, CAO Shengfei, TAN Jibo, WU Xinqiang, ZHANG Ziyu
图12 MAG焊接接头在人工海水中浸泡3年后的表面形貌[66]
Fig.12 Surface appearance (a) and roughness profile with laser displacement measurement (b) of coupon with f MAG weld joint after immersion in synthetic sea water for 3 a[66]