Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni合金热处理工艺优化及其高温高压水腐蚀行为研究
雷艾嘉, 戴训, 许江涛, 邓睿驹, 黄雪飞

Optimization of Heat Treatment Process and Corrosion Performance in High-temperature and High-pressure of Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni Alloy
LEI Aijia, DAI Xun, XU Jiangtao, DENG Ruiju, HUANG Xuefei
表2 腐蚀动力学曲线参数
Table 2 Corrosion kinetics parameters of Y1, Y3 and Zircaloy-4 alloys
SampleCorrosion mass gain at transition point / mg·dm-2Transition time / dKinetics law in the pre-transition regionR2
Zircaloy-435.61605.45t0.350.9984
Y143.22207.42t0.320.9983
Y345.02506.92t0.330.9983