Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni合金热处理工艺优化及其高温高压水腐蚀行为研究 |
雷艾嘉, 戴训, 许江涛, 邓睿驹, 黄雪飞 |
Optimization of Heat Treatment Process and Corrosion Performance in High-temperature and High-pressure of Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni Alloy |
LEI Aijia, DAI Xun, XU Jiangtao, DENG Ruiju, HUANG Xuefei |
图10 Y1合金和Y3合金高温高压水腐蚀不同时间后的金属-氧化物界面三维形貌 |
Fig.10 3D morphologies of the metal-oxide interfaces of Y1 alloy (a-e) and Y3 alloy (f-j) after exposure in high-temperature and high-pressure water for 70 d (a, f), 160 d (b, g), 220 d (c, h), 250 d (d, i), and 305 d (e, j) |
![]() |