Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni合金热处理工艺优化及其高温高压水腐蚀行为研究 |
雷艾嘉, 戴训, 许江涛, 邓睿驹, 黄雪飞 |
Optimization of Heat Treatment Process and Corrosion Performance in High-temperature and High-pressure of Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni Alloy |
LEI Aijia, DAI Xun, XU Jiangtao, DENG Ruiju, HUANG Xuefei |
图7 Y1合金高温高压水腐蚀不同时间后的表面氧化膜截面形貌 |
Fig.7 Cross-sectional morphologies of oxide films formed on Y1 alloy after exposure in high-temperature and high-pressure water for 70 d (a), 160 d (b), 220 d (c), 250 d (d), and 305 d (e) |
![]() |