Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni合金热处理工艺优化及其高温高压水腐蚀行为研究
雷艾嘉, 戴训, 许江涛, 邓睿驹, 黄雪飞

Optimization of Heat Treatment Process and Corrosion Performance in High-temperature and High-pressure of Zr-1.35Sn-0.22Fe-0.13Cr-0.05Ni Alloy
LEI Aijia, DAI Xun, XU Jiangtao, DENG Ruiju, HUANG Xuefei
图3 Y1合金和Y3合金基体的高角环形暗场(HAADF)图像
Fig.3 High-angle annular dark-field scanning (HAADF) images of Y1 alloy (a) and Y3 alloy (b)