污染海洋大气环境下不锈钢加速腐蚀试验环境谱评价及相关性
缪浩, 尹程辉, 王洪伦, 高逸晖, 陈俊航, 张昊, 李波, 吴俊升, 肖葵

Correlation of Laboratory Simulation Test and Field Exposure Test for Three Stainless Steels in Polluted Marine Atmosphere of Qingdao Coastal Area
MIAO Hao, YIN Chenghui, WANG Honglun, GAO Yihui, CHEN Junhang, ZHANG Hao, LI Bo, WU Junsheng, XIAO Kui
表3 430、316L和2205不锈钢极化曲线的拟合结果
Table 3 Fitting results of polarization curves of 430, 316L and 2205 stainless steels
MaterialTest time / hEcorr / mVIcorr / nA·cm-2
430107-489.421053.80
214-320.72309.34
321-190.0655.14
428-220.8282.78
316L107-49.75112.21
214-72.71104.07
321-186.53118.60
428-199.6271.19
2205107-114.06237.95
214-161.13100.26
321-221.0247.26
428-186.2565.60