污染海洋大气环境下不锈钢加速腐蚀试验环境谱评价及相关性 |
||||||||||||||||
缪浩, 尹程辉, 王洪伦, 高逸晖, 陈俊航, 张昊, 李波, 吴俊升, 肖葵 | ||||||||||||||||
Correlation of Laboratory Simulation Test and Field Exposure Test for Three Stainless Steels in Polluted Marine Atmosphere of Qingdao Coastal Area |
||||||||||||||||
MIAO Hao, YIN Chenghui, WANG Honglun, GAO Yihui, CHEN Junhang, ZHANG Hao, LI Bo, WU Junsheng, XIAO Kui | ||||||||||||||||
表2 430、316L和2205不锈钢室内加速试验后的拟合结果 |
||||||||||||||||
Table 2 Fitting results of 430, 316L and 2205 stainless steels after accelerated indoor testing |
||||||||||||||||
|
||||||||||||||||