污染海洋大气环境下不锈钢加速腐蚀试验环境谱评价及相关性 |
缪浩, 尹程辉, 王洪伦, 高逸晖, 陈俊航, 张昊, 李波, 吴俊升, 肖葵 |
Correlation of Laboratory Simulation Test and Field Exposure Test for Three Stainless Steels in Polluted Marine Atmosphere of Qingdao Coastal Area |
MIAO Hao, YIN Chenghui, WANG Honglun, GAO Yihui, CHEN Junhang, ZHANG Hao, LI Bo, WU Junsheng, XIAO Kui |
图10 试验428 h后的430、316L和2205不锈钢腐蚀产物的Fe2p分峰拟合图谱 |
Fig.10 Fe 2p fractional peak fitting spectra of corrosion products of 430 (a, b), 316L (c, d) and 2205 (e, f) stainless steels after corrosion for 428 h |
![]() |