退火工艺对304奥氏体不锈钢的组织演变及氢脆行为的影响 |
| 张慧云, 郑留伟, 梁伟 |
|
Effect of Annealing Process on Microstructure Evolution and Hydrogen Embrittlement Behavior of 304 Austenitic Stainless Steel |
| ZHANG Huiyun, ZHENG Liuwei, LIANG Wei |
| 图12 900 ℃-30 min和1000 ℃-60 min试样的氢解吸速率随温度变化曲线 |
| Fig.12 Hydrogen desorption rates of 900 oC-30 min and 1000 oC-60 min samples as a function of temperature |
|