退火工艺对304奥氏体不锈钢的组织演变及氢脆行为的影响 |
张慧云, 郑留伟, 梁伟 |
Effect of Annealing Process on Microstructure Evolution and Hydrogen Embrittlement Behavior of 304 Austenitic Stainless Steel |
ZHANG Huiyun, ZHENG Liuwei, LIANG Wei |
图9 700 ℃-5 min,700 ℃-10 min以及800 ℃-10 min试样的氢解吸速率随温度变化曲线 |
Fig.9 Hydrogen desorption rates of 700 oC-5 min, 700 oC-10 min and 800 oC-10 min samples as a function of temperature |
![]() |