退火工艺对304奥氏体不锈钢的组织演变及氢脆行为的影响 |
| 张慧云, 郑留伟, 梁伟 |
|
Effect of Annealing Process on Microstructure Evolution and Hydrogen Embrittlement Behavior of 304 Austenitic Stainless Steel |
| ZHANG Huiyun, ZHENG Liuwei, LIANG Wei |
| 图8 700 ℃-5 min,700 ℃-10 min以及800 ℃-10 min试样充氢前后的应力-应变曲线和氢脆敏感性 |
| Fig.8 Stress-strain curves of 700 oC-5 min, 700 oC-10 min and 800 oC-10 min samples before and after hydrogen charging (a), and their HE sensitivities (b) |
|