氢对2205双相不锈钢在3.5%NaCl溶液中缝隙腐蚀行为影响 |
| 汤熠鑫, 张飞, 崔中雨, 崔洪芝, 李燚周 |
|
Effect of Hydrogen on Crevice Corrosion Behavior of 2205 Duplex Stainless Steel in 3.5%NaCl Solution |
| TANG Yixin, ZHANG Fei, CUI Zhongyu, CUI Hongzhi, LI Yizhou |
| 图4 3.5%NaCl溶液中不同充氢时间下2205双相不锈钢的M-S曲线和载流子密度 |
| Fig.4 Mott-Schottky plots of the passive films formed on 2205 duplex stainless steel in 3.5%NaCl solution after hydrogen charging for different time: (a) Mott-Schottky plots, (b) carrier density |
|