掺氢环境下X80管线钢气相氢损伤研究
刘天乐, 韦博鑫, 付安庆, 苏航, 陈廷枢, 王超明, 王邃

Hydrogen Damage of X80 Pipeline Steel in Hydrogen-doped Gaseous Atmosphere
LIU Tianle, WEI Boxin, FU Anqing, SU Hang, CHEN Tingshu, WANG Chaoming, WANG Sui
表2 不同掺氢比条件下X80管线钢气相氢渗透动力学参数
Table 2 Kinetic parameters of gas-phase hydrogen permeation in X80 pipeline steel with different hydrogen doping ratios
Hydrogen blending ratio / %P / MPaD / m2·s-1Φ / mol·m-1·s-1·MPa-0.5
100.6251.19 × 10-106.43 × 10-11
301.8631.21 × 10-101.17 × 10-10
503.0061.21 × 10-101.99 × 10-10