重水堆压力管延迟氢化物开裂应力强度因子门槛值测试方法研究 |
| 鲍一晨, 石秀强, 孟凡江, 潘春婷, 明洪亮 |
|
Assessment Method of Threshold Stress Intensity Factor of Delayed Hydride Cracking for Pressure Tube in Heavy Water Reactor |
| BAO Yichen, SHI Xiuqiang, MENG Fanjiang, PAN Chunting, MING Hongliang |
| 图10 250 ℃下高倍断口形貌 |
| Fig.10 Fracture morphology observed at high magnification at 250 oC |
|