地下储氢库J55钢氢环境下微生物腐蚀机理研究 |
姜慧芳, 刘扬豪, 刘莹, 李迎超, 于浩波, 赵博, 陈曦 |
Mechanism of Microbial Corrosion of J55 Steel in Hydrogen-containing Environments in Underground Hydrogen Storage Facilities |
JIANG Huifang, LIU Yanghao, LIU Ying, LI Yingchao, YU Haobo, ZHAO Bo, CHEN Xi |
图6 不同条件下J55钢实验7 d后去除样品上腐蚀产物后最大点蚀坑的投影图像 |
Fig.6 2D projection image of the largest pitting pit for bacteria with square specimen (a), bacteria with U-bend specimen (b), bacteria with U-bend specimen + 0.22%H2 (c) and bacteria with U-bend specimen + 0.44%H2 (d) after 7 d |
![]() |