预充氢对Ni-Cr合金在高温高压水中腐蚀行为影响 |
| 白钲清, 农靖, 韦世宸, 徐健 |
|
Effect of Pre-charging Hydrogen on Corrosion Behavior of Ni-Cr Alloy in High Temperature and High Pressure Water |
| BAI Zhengqing, NONG Jing, WEI Shichen, XU Jian |
| 图3 预充氢条件下4种Ni-Cr合金在高温高压无氧水中浸泡720 h后表面SEM形貌 |
| Fig.3 SEM image of morphology of the corrosion products of 10Cr (a), 15Cr (b), 20Cr (c) and 30Cr (d) with pre-hydrogen charging after immersion in deoxidized HTHP water for 720 h |
|