激光增材制造AlCoCrFeNiSi高熵合金的氧化行为
郭静波, 杨守华, 周子翼, 牟仁德, 谢云, 舒小勇, 戴建伟, 彭晓

High-temperature Oxidation Behavior of Laser Additively Manufactured AlCoCrFeNiSi High Entropy Alloy
GUO Jingbo, YANG Shouhua, ZHOU Ziyi, MU Rende, XIE Yun, SHU Xiaoyong, DAI Jianwei, PENG Xiao
图5 不同激光功率沉积的Al0.21Co0.17Cr0.13Fe0.11Ni0.18Si0.20在“湿”空气中的氧化增重曲线及氧化增重平方随时间的变化曲线
Fig.5 Oxidation kinetics (a) and corresponding parabolic plots (b) of Al0.21Co0.17Cr0.13Fe0.11Ni0.18Si0.20 fabricated by LMD at different laser powers during 20 h exposure to wet air at 1100 oC