预氧化GH4169合金在中温固态NaClO2 + H2O气氛中的腐蚀行为研究
张伟东, 崔宇, 刘莉, 王福会

Corrosion Behavior of Pre-oxidized GH4169 Alloy Beneath Solid NaCl Deposit Film in Wet Oxygen Flow at 600 oC
ZHANG Weidong, CUI Yu, LIU Li, WANG Fuhui
图10 经10 h预氧化的GH4169合金表面涂覆NaCl后在600 ℃ O2 + H2O气氛下腐蚀不同时间形成的氧化膜内元素分布
Fig.10 Element mappings of the oxide scale formed on 10 h pre-oxidized GH4169 alloy with solid NaCl deposit after exposure in wet O2 + H2O at 600 oC for 1 h (a), 3 h (b) and 5 h (c)