预氧化GH4169合金在中温固态NaCl和O2 + H2O气氛中的腐蚀行为研究 |
张伟东, 崔宇, 刘莉, 王福会 |
Corrosion Behavior of Pre-oxidized GH4169 Alloy Beneath Solid NaCl Deposit Film in Wet Oxygen Flow at 600 oC |
ZHANG Weidong, CUI Yu, LIU Li, WANG Fuhui |
图9 经10 h预氧化的GH4169合金表面涂覆NaCl后在600 ℃ O2 + H2O气氛下腐蚀5 h的TEM分析结果 |
Fig.9 TEM analysis results of microstruture and phase composition of the oxide scale formed on 10 h pre-oxidized GH4169 alloy with NaCl deposit after exposure in O2 + H2O at 600 oC for 5 h |
![]() |