预氧化GH4169合金在中温固态NaClO2 + H2O气氛中的腐蚀行为研究
张伟东, 崔宇, 刘莉, 王福会

Corrosion Behavior of Pre-oxidized GH4169 Alloy Beneath Solid NaCl Deposit Film in Wet Oxygen Flow at 600 oC
ZHANG Weidong, CUI Yu, LIU Li, WANG Fuhui
图7 经10 h预氧化的GH4169合金在600 ℃下表面涂覆NaCl和O2 + H2O气氛下腐蚀1 h后TEM分析结果
Fig.7 Cross-sectional image and electron diffraction patterns (a) of the oxide scale formed on 10 h pre-oxidized GH4169 alloy with solid NaCl deposit after exposure in O2 + H2O at 600 oC for 1 h, and depth profile of Cl ions (b)