预氧化GH4169合金在中温固态NaCl和O2 + H2O气氛中的腐蚀行为研究 |
张伟东, 崔宇, 刘莉, 王福会 |
Corrosion Behavior of Pre-oxidized GH4169 Alloy Beneath Solid NaCl Deposit Film in Wet Oxygen Flow at 600 oC |
ZHANG Weidong, CUI Yu, LIU Li, WANG Fuhui |
图1 GH4169 合金在900 ℃预氧化10 h后表面形貌和相分析结果 |
Fig.1 SEM surface morphology (a), cross-section morphology (b), and XRD pattern (c) of GH4169 alloy after 10 h oxidation at 900 oC |
![]() |