DD6单晶Ni基高温合金表面CVD渗Al涂层的氧化行为 |
许习文, 舒小勇, 陈智群, 何海瑞, 董舒赫, 房雨晴, 彭晓 |
Oxidation Behavior of CVD Aluminized Coatings on DD6 Single Crystal Ni-based Superalloy |
XU Xiwen, SHU Xiaoyong, CHEN Zhiqun, HE Hairui, DONG Shuhe, FANG Yuqing, PENG Xiao |
图8 两种CVD渗Al涂层在1000 ℃空气中短时氧化2 h后的表面形貌 |
Fig.8 Surface morphologies of Al2O3 scales formed on CVD aluminized Ni (a) and DD6 superalloy (b) after short-term oxidation of 2 h in air at 1000 oC |
![]() |