DD6单晶Ni基高温合金表面CVD渗Al涂层的氧化行为 |
| 许习文, 舒小勇, 陈智群, 何海瑞, 董舒赫, 房雨晴, 彭晓 |
|
Oxidation Behavior of CVD Aluminized Coatings on DD6 Single Crystal Ni-based Superalloy |
| XU Xiwen, SHU Xiaoyong, CHEN Zhiqun, HE Hairui, DONG Shuhe, FANG Yuqing, PENG Xiao |
| 图5 两种CVD渗Al涂层在1000 ℃空气中氧化 20 h后的表面形貌 |
| Fig.5 Surface morphologies of CVD aluminized coatings on Ni (a, b) and DD6 superalloy (c, d) after 20 h oxidation in air at 1000 oC |
|