典型氟橡胶密封材料热空气老化试验研究 |
刘明, 张连栋, 孙志华, 高蒙, 闫巍, 赵明亮 |
Assessment on Performance Decay Induced by Hot Air Aging for Typical Fluoroelastomer Sealing Materials |
LIU Ming, ZHANG Liandong, SUN Zhihua, GAO Meng, YAN Wei, ZHAO Mingliang |
图7 热空气环境下氟橡胶不同温度下老化77 d后拉伸断口形貌 |
Fig.7 Tensile fracture morphologies of fluoroelastomer FX-17 after hot air aging for 77 d at 200 oC (a, b) and 220 oC (c, d) |
![]() |