典型氟橡胶密封材料热空气老化试验研究 |
刘明, 张连栋, 孙志华, 高蒙, 闫巍, 赵明亮 |
Assessment on Performance Decay Induced by Hot Air Aging for Typical Fluoroelastomer Sealing Materials |
LIU Ming, ZHANG Liandong, SUN Zhihua, GAO Meng, YAN Wei, ZHAO Mingliang |
图6 典型氟橡胶FX-17在240 ℃下热空气老化不同周期后的拉伸断口形貌 |
Fig.6 Tensile fracture morphologies of typical fluoroelastomer FX-17 after hot air aging at 240 oC for 0 d (a, b), 7 d (c, d), 35 d (e, f) and 77 d (g, h) |
![]() |