Pt改性共晶高熵合金AlCoCrFeNi2.1 热腐蚀行为研究 |
| 黄勤英, 李彧卓, 阳颖飞, 任盼, 王启伟 |
|
Hot Corrosion Behavior of Pt Modified AlCoCrFeNi2.1 Eutectic High Entropy Alloy |
| HUANG Qinying, LI Yuzhuo, YANG Yingfei, REN Pan, WANG Qiwei |
| 图11 两种样品在900 ℃下混合盐(Na2SO4 + NaCl)中热腐蚀100 h的形貌 |
| Fig.11 Macro-morphologies of YHf-EHEA (a) and YHfPt-EHEA (b, c) after 100 h of hot corrosion in the mixed salt (Na2SO4 +NaCl) at 900 oC |
|