Pt改性共晶高熵合金AlCoCrFeNi2.1 热腐蚀行为研究 |
黄勤英, 李彧卓, 阳颖飞, 任盼, 王启伟 |
Hot Corrosion Behavior of Pt Modified AlCoCrFeNi2.1 Eutectic High Entropy Alloy |
HUANG Qinying, LI Yuzhuo, YANG Yingfei, REN Pan, WANG Qiwei |
图3 两种样品在800 ℃下混合盐(Na2SO4 + K2SO4)中热腐蚀200 h后的表面氧化膜形貌 |
Fig.3 Surface morphologies of YHf-EHEA (a, b) and YHfPt-EHEA (c, d) after hot corrosion for 200 h in mixed salt (Na2SO4 + K2SO4) at 800 oC |
![]() |