两种热处理状态的镍基单晶高温合金在900℃下(Na2SO4 + NaCl)混合盐中热腐蚀行为研究 |
张金龙, 付广艳, 宁礼奎, 刘恩泽, 谭政, 佟健, 郑志 |
Hot Corrosion Behavior of a Nickel Based Single Crystal High Temperature Alloy Subjected to Different Heat Treatments |
ZHANG Jinlong, FU Guangyan, NING Likui, LIU Enze, TAN Zheng, TONG Jian, ZHENG Zhi |
图7 CH合金样品在900℃腐蚀100 h后的SEM形貌及EDS图谱 |
Fig.7 SEM morphology of CH sample after hot corrosion at 900oC for 100 h (a), and corresponding EDS mappings of Al (b), O (c), Cr (d), Ni (e), Co (f), Re (g) and S (h) |
![]() |