T2铜合金和Q235钢在模拟北山地下水环境中的电偶腐蚀行为研究
庞洁, 刘相局, 刘娜珍, 侯保荣

Galvanic Corrosion of T2 Cu-alloy and Q235 Steel in Simulated Beishan Groundwater Environment
PANG Jie, LIU Xiangju, LIU Nazhen, HOU Baorong
图7 25℃时不同Cl-浓度下面积比为10∶1时Q235钢表面腐蚀后SEM形貌图
Fig.7 SEM surface morphologies of Q235 steel after corrosion at 25oC under the conditions of the area ratio of 10∶1 and Cl- concentrations of 0.001 mol·L-1 (a, b), 0.05 mol·L-1 (c, d), and 2 mol·L-1 (e, f)