Ti45Al8.5Nb合金表面Zr-SiO2 复合涂层的制备及其抗高温氧化性能研究
吴亮亮, 殷若展, 陈朝旭, 梁君岳, 孙擎擎, 伍廉奎, 曹发和

Preparation and High Temperature Oxidation Resistance of Zr-SiO2 Composite Coating on Ti45Al8.5Nb Alloy
WU Liangliang, YIN Ruozhan, CHEN Zhaoxu, LIANG Junyue, SUN Qingqing, WU Liankui, CAO Fahe
图8 经900℃, 100 h氧化的SiO2涂层的表面Raman光谱, 以及相同条件氧化后的Zr-SiO2复合涂层的表面光学形貌与标记点1和2处的Raman光谱
Fig.8 Raman spectrum (a), optical surface morphology (b) and Raman spectra of the marked positions 1 (c) and 2 (d) in Fig.8b for SiO2 coating (a) and Zr-SiO2 composite coating (b-d) after oxidation at 900oC for 100 h