潮湿空气中应力耦合固态NaCl作用下GH4169合金的中温腐蚀行为研究 |
王文泉, 崔宇, 薛蕴鹏, 刘莉, 王福会 |
Corrosion Behavior of GH4169 Alloy Under Flexural Tensile Stress and Beneath a NaCl Deposit Film in Water Vapor Containing Air at 600oC |
WANG Wenquan, CUI Yu, XUE Yunpeng, LIU Li, WANG Fuhui |
图9 振动抛光后的标准制度热处理GH4169合金内腐蚀形貌 |
Fig.9 Internal corrosion morphologies of standard heat-treated GH4169 alloy under a stress load of 0 MPa (a, d), 600 MPa (b, e) and 800 MPa (c, f) after shock polishing: (a-c) backscattered electron image of the internal corrosion morphologies, (d-f) internal corrosion morphologies with high contrast |
![]() |