煤灰中碱金属硫酸盐和氯盐含量对HR3C和渗铝HR3C不锈钢腐蚀行为的影响 |
喻政, 陈明辉, 王金龙, 杨莎莎, 王福会 |
Influence of Alkali Metal Sulfate- and Chloride-salts Content in Artificial Coal Ash on Corrosion Behavior of HR3C Steels With and Without Aluminizing |
YU Zheng, CHEN Minghui, WANG Jinlong, YANG Shasha, WANG Fuhui |
图1 A-HR3C的表面、截面形貌和HR3C的表面形貌及对应的XRD谱 |
Fig.1 Surface (a) and cross-sectional (b) morphologies of A-HR3C, surface morphology of HR3C (c), and corresponding XRD patterns of A-HR3C and HR3C surface (d) |
![]() |