螺纹钢中MnS夹杂物诱发的局部腐蚀行为 |
韩宇龙, 李健, 郭丽雅, 杨边疆, 陆恒昌, 韦习成, 董瀚 |
Localized Corrosion Behavior Induced by MnS Inclusions in HRB400E Rebar Steel |
HAN Yulong, LI Jian, GUO Liya, YANG Bianjiang, LU Hengchang, WEI Xicheng, DONG Han |
图4 团簇与单一夹杂物浸泡60 min后的SEM图和3D轮廓图 |
Fig.4 SEM images (a, b) and 3D profilometer images (c) of the clustered (a, b, c1) and single (a, b, c2) inclusions not immersed (a1) and immersed for 15 min (a2), 30 min (b1) and 60 min (b2) |
![]() |