螺纹钢中MnS夹杂物诱发的局部腐蚀行为 |
| 韩宇龙, 李健, 郭丽雅, 杨边疆, 陆恒昌, 韦习成, 董瀚 |
|
Localized Corrosion Behavior Induced by MnS Inclusions in HRB400E Rebar Steel |
| HAN Yulong, LI Jian, GUO Liya, YANG Bianjiang, LU Hengchang, WEI Xicheng, DONG Han |
| 图3 尺寸约为60.5 μm2的MnS夹杂物浸泡60 min时SEM-EDS图 |
| Fig.3 SEM-EDS images of the MnS (~60.5 μm2) inclusions in HRB400E steel unimmersed (a) and immersed for 15 min (b), 30 min (c) and 60 min (d) |
|