电泳沉积制备MnCo尖晶石涂层的高温长期稳定性研究 |
王碧辉, 刘聚, 崔志翔, 肖博, 杨天让, 张乃强 |
Long-term Stability of MnCo Spinel Coatings Prepared by Electrophoretic Deposition at High Temperatures |
WANG Bihui, LIU Ju, CUI Zhixiang, XIAO Bo, YANG Tianrang, ZHANG Naiqiang |
图4 Mn1.5Co1.5O4/SUS430和Mn1.5Co1.5O4/Crofer22H两种试样在不同温度下氧化1000 h后的截面形貌及元素分布图(图中黄线标记为含Cr氧化层厚度) |
Fig.4 Cross-sectional morphologies and elemental line of Mn1.5Co1.5O4/SUS430 (a-c) and Mn1.5Co1.5O4/Crofer22H (d-f) after oxidation for 1000 h at 800oC (a, d), 750oC (b, e) and 700oC (c, f) (the thicknesses of Cr-containing oxide layers are shown in the insets) |
![]() |