1050A铝合金在山东不同典型环境中的大气腐蚀行为特征研究 |
樊志彬, 高智悦, 宗立君, 吴亚平, 李辛庚, 姜波, 杜宝帅 |
Corrosion Behaviour and Characteristics of 1050A Al-alloy Exposed in Typical Atmospheres of Shandong Province |
FAN Zhibin, GAO Zhiyue, ZONG Lijun, WU Yaping, LI Xingeng, JIANG Bo, DU Baoshuai |
图1 1050A铝合金在青岛、东营、威海及潍坊大气环境中暴晒宏观腐蚀形貌 |
Fig.1 Macroscopic morphologies of the front (a1-h1) and back (a2-h2) surfaces of 1050A Al-alloy samples after atmospheric exposure in Qingdao (a, b), Dongying (c, d), Weihai (e, f) and Weifang (g, h) for 12 months (a, c, e, g) and 42 months (b, d, f, h) |
![]() |