1, 2, 4-三唑在模拟调相机转子内冷却水中对铜的缓蚀作用
冯礼奎, 程一杰, 宋小宁, 于志勇, 严梓轩, 张大全

Corrosion Inhibition of 1, 2, 4-triazaole on Copper in a Stimulated Cooling Water for Synchronous Condenser
FENG Likui, CHENG Yijie, SONG Xiaoning, YU Zhiyong, YAN Zixuan, ZHANG Daquan
表3 TAZ在样品表面的成膜厚度及参数
Table 3 Thicknesses of TAZ films adsorbed on Cu

TAZ

mmol·L-1

Goodness of Fitting (GOF)Mean Square Error (MSE)

Thickness

of TA2

nm

20.999992.46428.78
50.999965.11667.86
100.999955.64808.64
150.9998210.5888.76
200.999366.59128.87