CCSAQ235B钢在长江淡水环境中腐蚀行为研究
张照易, 周学杰, 陈昊, 吴军, 陈志飈, 陈志坚

Corrosion Behavior of Two Steels CCSA and Q235B in Changjiang Freshwater Surroundings
ZHANG Zhaoyi, ZHOU Xuejie, CHEN Hao, WU Jun, CHEN Zhibiao, CHEN Zhijian
表3 CCSA和Q235B钢在长江淡水环境腐蚀失重拟合结果
Table 3 Fitting results of mass losses of CCSA and Q235B steels in Changjiang freshwater environments
MaterialAreamnR2Fitting formula
CCSAAtmosphere0.019640.409640.95912C = 0.01964T0.40964
Waterline0.106660.721590.97966C = 0.10666T0.72159
Underwater0.063690.643840.98483C = 0.06369T0.64384
Q235BAtmosphere0.021640.420720.95678C = 0.02164T0.42072
Waterline0.108080.733980.98666C = 0.10808T0.73398
Underwater0.064570.654540.98972C = 0.06457T0.65454