外加电位下Ag/Sn电偶的腐蚀行为 |
戴威, 刘园园, 涂闻芮, 孙阳庭, 李劲, 蒋益明 |
Corrosion Behavior of Ag/Sn Galvanic Couple at Applied Potential |
DAI Wei, LIU Yuanyuan, TU Wenrui, SUN Yangting, LI Jin, JIANG Yiming |
图5 Sn在0.01 mol/L NaCl溶液中极化曲线测试后的形貌和SEM/EDS表征 |
Fig.5 Optical image (a), SEM images (b, f), element distribution maps of Fig.5b (c‒e) and EDS result of points in Fig.5f (g, h) of Sn after polarization in 0.01 mol/L NaCl solution |
![]() |