不同植酸盐对Q235钢腐蚀行为的影响
周龙, 鲁骏, 丁文珊, 李昊, 陶涛, 师超, 邵亚薇, 刘光明

Effect of Different Phytates on Corrosion Behaviors of Carbon Steel
ZHOU Long, LU Jun, DING Wenshan, LI Hao, TAO Tao, SHI Chao, SHAO Yawei, LIU Guangming
图8 Q235钢在磷酸锌、植酸锌、植酸钙、植酸锰、植酸铝浸出液中浸泡不同时间后的表面形貌