Inconel 718及其渗铝涂层在Na2SO4 + 5%NaCl混合盐膜下的热腐蚀行为
胡琪, 耿树江, 王金龙, 王福会, 孙清云, 吴勇, 夏思瑶

Hot Corrosion Behavior of Inconel 718 Without and With Aluminide Coating in Air Beneath a Thin Film of Salt Mixture of Na2SO4 + 5%NaCl
HU Qi, GENG Shujiang, WANG Jinlong, WANG Fuhui, SUN Qingyun, WU Yong, XIA Siyao
表2 对应图6不同区域的EDS分析 (atomic fraction / %)
Table 2 EDS analysis results of the different regions marked in Fig.6
PositionOAlCrFeNiNbMoTiS
H63.112.098.2314.603.935.23-2.81-
I53.44-3.8032.4010.36----
J71.791.520.7719.166.76----
K56.0030.341.351.289.63---1.40
L66.9925.772.280.451.18---3.33
M68.180.9925.210.492.351.620.130.780.25
N8.990.622.5117.0365.130.624.99-0.11
O67.0319.292.823.277.29--0.250.05
P58.1638.091.560.610.98--0.330.27
Q63.210.545.0117.4012.281.00-0.56-
R55.6738.814.080.440.57-0.410.02
S67.0628.451.930.911.45----